SAE AMS 4983C-2002 钛合金锻件10V - 2FE - 3AL消耗电极熔化,处理单步固溶热处理和老化180 KSI ( 1241 MPA )抗拉强度
SAE AMS 4983C-2002 标准详情
- 标准号:SAE AMS 4983C-2002
- 中文标题:钛合金锻件10V - 2FE - 3AL消耗电极熔化,处理单步固溶热处理和老化180 KSI ( 1241 MPA )抗拉强度
- 英文标题:titanium alloy, forgings 10v - 2fe - 3al consumable electrode melted, single-step solution heat treated and aged 180 ksi (1241 mpa) tensile strength
- 标准类别:美国汽车工程师协会标准SAE
- 发布日期:2002-10-01
内容简介
This specification covers a titanium alloy in the form of forgings under 1.00 inch (25 mm) in nominal cross-sectional thickness and of forging stock. These forgings have been used typically for parts in high stress and stress-corrosion-resistant appl